| HEAVYGAUGE SOFFIT |
| TypicalPhysical Properties |
| TEST |
STANDARD METHOD |
UNIT OF MEASURE |
RESULT |
| IZODimpact (23°C/73°F) |
ASTM D-256 |
ft-lb/in |
2.4 |
| Tensilestrength |
ASTM D-638 |
Psi |
>6000 |
| Modulusof elasticity |
ASTM D-638 |
Psi |
>365,000 |
| Deflectiontemperature under load @ 264 Psi |
ASTM D-648 |
°F
|
170 |
| Coefficientof linear expansion |
ASTM E-831 |
105in/in/°F |
3.07 |
| Chemicalresistance |
ASTM D-543 |
|
Excellent |
| Cellclassification |
ASTM D-1784 |
Class# |
1334434 |
| Compoundclass |
ASTM D-3679 |
Class# |
2 |
| Siding/ExtrudateTypical Physical Properties |
| TEST |
STANDARD METHOD |
UNIT OF MEASURE |
RESULT |
Impactresistance (23°C/73°F)
|
ASTMD-4226 |
in-lb/mil |
2.75 |
| Impactresistance (0°C/32°F) |
ASTMD-4226 |
in-lb/mil |
1.95 |
| Lowtemperature flexibility |
CAN/CGSB41- 24-95 |
% passed |
>80 |
| Shrinkage/reversion |
ASTMD-3679-95 |
% |
<3.0 |
| Surface distortion(oil can) |
ASTMD-3679-95 |
°F |
>150 |
| Nominalthickness |
CAN/CGSB41- 24-95 |
mm |
1.17 |
| Wallthickness |
ASTM D-3679-95 |
inch |
0.046 |
| FireCharacteristics |
| TEST |
STANDARD METHOD |
RESULT |
Flamespread index
Fuel contribution
Smoke developed index
|
ASTM E84, UBC 42-1 |
18
0
<450 |
| Self-ignitiontemperature, °F |
ASTMD-1929, UBC 52-3 |
810 |
Smokedensity rating (%)
Maximum smoke density (%)
Visibility of exit sign |
ASTMD-2843, UBC 52-2 |
42.1
56.0
Good |
Totalburn time, seconds
Extent of burning, mm
Fire resistance rating |
ASTMD-635
ASTM D-635
ASTM E-119 |
<5
<5
1 hour |
| TRADITIONALSOFFIT |
| TypicalPhysical Properties |
| TEST |
STANDARD METHOD |
UNIT OF MEASURE |
RESULT |
| IZODimpact (23°C/73°F) |
ASTM D-256 |
ft-lb/in |
2.4 |
| Tensilestrength |
ASTM D-638 |
Psi |
>6000 |
| Modulusof elasticity |
ASTM D-638 |
Psi |
>365,000 |
| Deflectiontemperature under load @ 264 Psi |
ASTM D-648 |
°F
|
170 |
| Coefficientof linear expansion |
ASTM E-831 |
105in/in/°F |
3.07 |
| Chemicalresistance |
ASTM D-543 |
|
Excellent |
| Cellclassification |
ASTM D-1784 |
Class# |
1334434 |
| Compoundclass |
ASTM D-3679 |
Class# |
2 |
| Siding/ExtrudateTypical Physical Properties |
| TEST |
STANDARD METHOD |
UNIT OF MEASURE |
RESULT |
Impactresistance (23°C/73°F)
|
ASTMD-4226 |
in-lb/mil |
2.35 |
| Impactresistance (0°C/32°F) |
ASTMD-4226 |
in-lb/mil |
1.71 |
| Lowtemperature flexibility |
CAN/CGSB41- 24-95 |
% passed |
>80 |
| Shrinkage/reversion |
ASTMD-3679-95 |
% |
<3.0 |
| Surface distortion(oil can) |
ASTMD-3679-95 |
°F |
>150 |
| Nominalthickness |
CAN/CGSB41- 24-95 |
mm |
1.07 |
| Wallthickness |
ASTM D-3679-95 |
inch |
0.042 |
| FireCharacteristics |
| TEST |
STANDARD METHOD |
RESULT |
Flamespread index
Fuel contribution
Smoke developed index
|
ASTM E84, UBC 42-1 |
18
0
510.2 |
| Self-ignitiontemperature, °F |
ASTMD-1929, UBC 52-3 |
810 |
Smokedensity rating (%)
Maximum smoke density (%)
Visibility of exit sign |
ASTMD-2843, UBC 52-2 |
42.1
56.0
Good |
Totalburn time, seconds
Extent of burning, mm
Fire resistance rating |
ASTMD-635
ASTM D-635
ASTM E-119 |
<5
<5
1 hour |
Warranty
 |
We’vegot you COVERED.
Royal offers an exclusive lifetime, non-prorated,fully transferable to lifetime non-prorated limitedwarranty with the exclusive Dura™ Color Protection.

|
 |
Color That's Guaranteed
The innovative Royalside™ Compound formulationdelivers superior durability in color throughthe most advanced color technology available.
Should color fade beyond what is specified inthe Royal warranty, your vinyl siding will bereplaced (includes material and labor).
GUARANTEED
|
| |
Warranty documentation is provided for downloadin PDF format. You will need Adobe Acrobat Readerto view or print.
 |
Installation Guide